Powder Metallurgy Case Study Part Image - MIM Connector

MIM Connector

Finished Weight of Component :
Density (g/cm3) :

Tensile Strenght (N/mm2) :

Yield Strength (=0.2% N/mm2) :

Hardness :
Treatment :
Description: This complex MIM connector is made from high strength, high corrosion resistant stainless steel powder (Schunk Material Specification: No. 1.4028 (X30Cr13)) which is supplied to the end-user in a heat treated (hardened and tempered) condition.

Company: Schunk Sintermetalltechnik GmbH

  Rodheimer Str 59, Heuchelheim Germany, D-35452
Tel  +49 641 608 1565
Fax  +49 641 608 1488
E-mail:   dieter.born@schunk-group.com
Contact:  Mr. Dieter Born
Web: www.schunk-group.com