| Potentiometer

Finished Weight of Component :
Density (g/cm3) :
Tensile Strenght (N/mm2) : 759Mpa
Yield Strength (=0.2% N/mm2) :
Hardness :
Treatment :
Description: Two PM steels and a PM 316L stainless steel limit striker are used in this Potentiometer. The smoller gear is made from copper-nickel steel material and is heat treated, ist has tensible strength of 759Mpa. The larger gear is made from the same material and has tensile strength of 697 Mpa. The limit striker has a tensile strength of 297 Mpa.
|